Case-Hardened or Through-Hardened: How to Decide Before You Source

The same gear drawing goes out to three shops and comes back with three different heat treatments. One quotes carburize, quench and grind.

Case-Hardened or Through-Hardened: How to Decide Before You Source

The same gear drawing goes out to three shops and comes back with three different heat treatments. One quotes carburize, quench and grind. Another quotes quench and temper, then finish machine. The price gap is around thirty percent and the lead time gap is a month. Buyers usually take the cheaper one, and only find out at commissioning — when the housing is noisy and the flanks are pitting — that the decision was never about money. It was about which hardness structure the tooth actually needs.

The difference between the two routes is where the hardness sits. Carburizing takes a low-carbon alloy steel such as 20CrMnTi or 20CrMo, adds carbon to the surface layer, and quenches it. The result is a case of roughly 0.5 to 3.0 mm at 58-62 HRC over a core that stays in the 30-42 HRC range. Through-hardening goes the other way: 42CrMo is quenched through and tempered back to 269-321 HB, one hardness from surface to centre; 40Cr lands at 241-286 HB after tempering. The carburized route splits wear resistance and toughness into two layers. The second asks one hardness to do both jobs.

Why a gear wants that split comes down to two different failures. The flank sees rolling contact stress with sliding, and if the surface is not hard enough it pits and spalls. The root sees alternating bending tensile stress, and if the core is hard and brittle, a crack that starts there ends the part. Carburizing separates the two requirements, which is why a carburized gear of the same size carries more torque. Through-hardening is a compromise in both directions: raise the bulk hardness and wear improves while core toughness drops; soften it and the root is safe while the flank gives up.

The process chain matters more to lead time and cost than the hardness number does. A carburized gear runs a long route — forge, normalize, rough turn, hob, carburize and quench — and the distortion that comes out of the furnace has to be cut away by grinding. That means grinding stock has to be right: too little and black patches stay on the flank, too much and grinding burn becomes a risk. Done properly, hard finishing holds DIN 4-5, equivalent to ISO 4-5, and keeps noise and backlash under control. A through-hardened gear runs a shorter route — rough turn, quench and temper, finish turn, hob or shape — with heat treatment ahead of finish machining, so dimensions stay put and no hard grinding is needed. The accuracy ceiling is set by the tool and the cutting parameters, and in normal production it lands between grade 5 and grade 7. Holding grade 6 or better in a through-hardened gear is a matter of machine condition and process discipline, not of paying more.

There are two intermediate routes worth knowing. Induction hardening after quench and tempering heats only the tooth region, to a depth of 1.0-5.0 mm at 48-58 HRC, leaves the core untouched, and keeps distortion small; on large modules it is often the practical answer. Nitriding goes further in the other direction: 42CrMo or 38CrMoAl at 500-570 °C gives 900-1100 HV over 0.1-0.6 mm, with dimensional change small enough that no further machining is normally required. The limit is case depth — a thin nitrided layer will not carry heavy contact stress.

Selection comes down to a handful of parameters pulling against each other: module, tooth count, centre distance, transmitted torque, speed and pitch line velocity, shock level, accuracy grade, batch size, and whether hard grinding is available downstream. Large module, few teeth, high torque — the case depth has to grow with it, cycle time grows, distortion grows, and quench-and-temper plus induction hardening often wins on total cost. Small module, high speed, low noise — hard finishing is close to the only way to get there. Above roughly 20 m/s pitch line velocity the dynamic load on the flank rises, and a soft through-hardened surface struggles to stay stable. On large single pieces the furnace may not take the part and press-quench tooling cannot be amortised, at which point carburizing stops being a real option.

One more layer gets skipped in most purchase orders: steel cleanliness. A Gear Solutions article by D. Scott MacKenzie published on 14 October 2026 sets out the mechanism plainly. Non-metallic inclusions create local stress concentrations that initiate tooth-root bending fatigue, contact-fatigue spalling and heat-treatment cracking. The article works through the four ASTM E45 inclusion types. Type C silicate stringers are specifically noted as reducing bending fatigue life in a through-hardened gear, because the stressed volume extends farther into the tooth section; in a carburized gear the same inclusion is most troublesome near the effective-case-depth transition, where it meets a steep hardness and residual-stress gradient. A heat of steel that passes on a carburized part will not necessarily pass on a through-hardened one. Writing “42CrMo” on the drawing is not a material specification. Inclusion rating and acceptance criteria belong in the technical agreement, and AGMA 923-C22 defines what those ratings should be for different gear grades.

At Geyontech both routes run in-house. Carburized 20CrMnTi goes through hardening and grinding to DIN 4-5, equivalent to ISO 4-5. Through-hardened 42CrMo is hobbed to DIN 4 on single parts and DIN 5 in series. Profile, lead and accumulated pitch are checked on a P400 and a Klingelnberg P26, complex contours go to a Zeiss CMM, and flank hardness is sampled on a Rockwell tester.

So the question is not whether carburizing beats through-hardening, and not whether the cheaper quote is good enough. Write down load, speed, accuracy and batch size down before choosing the tooth structure, and agree the price after that. Reversed, the saving comes back on the assembly line.

Send the drawing, the material grade, the accuracy requirement and the batch size, and we will come back with one clear route for that tooth: https://www.geyontech.com/get-a-gear-quote/

(Source: Gear Solutions, “Steel cleanliness in gears”, D. Scott MacKenzie, 14 October 2026, https://gearsolutions.com/departments/hot-seat/steel-cleanliness-in-gears/ )

Send us a drawing — get engineering feedback first

Upload a 2D/3D drawing (STEP, DXF, PDF) — we reply with a quote and lead time.